Physical Properties:
Density: 8.14g/cm3
Melting Point: 1370-1400 °C
Modulus of Elasticity: 193 kN/mm2
Thermal Conductivity:12.3 λ/(W(m•℃)Hardness:HB≤200
Electrical Resistivity( 21- 93°C): 14μ m/m °C
Approx Service Temperature: -200 to +250°C
Main Characteristics:Good reduction, oxidation and nitridize media resistance, great metallurgical stability at long time high temperature.Applications:Mainly applied in heat exchanger, high temperature heater and cracking furnace tubes used in chemical, electricity generating, petrochemical industries.
Specification:Forgings,Rod, Plate, Strip,Ring, Wire, Bolts, Springs and other consultations supply, according to customer's production
Chemical Compositions:
Chemical Compositions(%)
|
C
|
Cr
|
Ni
|
Mo
|
Fe
|
Al
|
Cu
|
Mn
|
Si
|
P
|
S
|
Ti
|
≤
0.05
|
19.5
-
23.5
|
38
-
46
|
2.5
-
3.5
|
rem
|
≤
0.20
|
1.5
-
3.0
|
≤
1.0
|
≤
0.50
|
≤
0.03
|
≤
0.03
|
0.6
-
1.2
|